WinSperse 5170


               

WinSperse 5170

Pigment modifier for solvent based applications

 Chemical composition

 General application guidance

 Mid-to-low polar low molecular weight polymer with pigment affinity groups

 Use 3-8% on dry pigment basis.

 Add 4 part of Winsperse 5170 and 2 part of acetic acid to 20X water to dissolve before use.

 Chemo-physical Properties

 Application tips

 Appearance: yellowish solid

 Active ingredient: 100%

 Amine value(mgKOH/g): 180-200

 Density(g/ml,40℃): 0.87-0.89

 For  making  P.Y.13,  P.Y.14,P.Y.83, add 3-8% WinSperse5170 to the coupling solution,when the reaction temperature heated  up,  add  5-10% WinSperse 2020. Such modified pigment is used in nitrocellulose systems  to  improve  color strength, gloss, viscosity and

storage stability.

 For P.B.15:3 cake, add 6-10% sulphonated  phthalocyanine while stiring, heat the mixture to 60-70℃, add WinSperse 5170 10-15%, continuing stiring for

2 hours, filtrate and bake to dry to obtain P.B.15:4 for use in solvent based ink especially in nitrocellulose systems.

 Characteristics

 Package

 Especially well suited to modify pigment  used  in  nitrocellulose systems for better viscosity and storage stability with higher color strength and gloss.

 Drum: 17kg/drum

 Application scope

 Storage

 Organic pigment

 Store in cool and dry places,good for 2 year.